Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 64.0 GPa | 9280 ksi | |
Schott Glass 8250 Borosilicate Glass Borosilicate glass for sealing to Kovar metal and molybdenum, electrically highly insulating, low refractive index, good insulator X-ray tubes, transmitting tubes, image amplifier tubes, He-Ne-lase.. |
|||
Modulus of Elasticity | 64.0 GPa | 9280 ksi | |
Schott Glass 8270 Borosilicate Glass Borosilicate glass for sealing to Kovar metal and molybdenum, electrically highly insulating, defined UV absorption, stabilized against solarization Backlights The heavy metal content for the elem.. |
|||
Modulus of Elasticity | 64.0 GPa | 9280 ksi | |
Schott Glass 8688 Borosilicate Glass Borosilicate glass, highly UV-blocked, stabilized against solarization, sealing glass to Tungsten Backlights The heavy metal content of the elements lead, cadmium, mercury, and hexavalent chromium.. |
|||
Modulus of Elasticity | 64.0 GPa | 9280 ksi | |
Schott SF10 Glass Information Provided by SCHOTT North America, Inc. |
|||
Modulus of Elasticity | 64.0 GPa @Temperature 1200 °C |
9280 ksi @Temperature 2190 °F |
|
ATI Wah Chang Nb/Nb Alloy C-103 This alloy satisfies most rocket engine applications for temperatures up to 2700°F because of superior mechanical properties at all temperatures. Offers weight savings over many rocket engine desig.. |