Polymer Property : Modulus of Elasticity = 57.0 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 57.0 GPa
8270 ksi
Schott F2 Glass
Information Provided by SCHOTT North America, Inc.
Modulus of Elasticity 57.0 GPa
8270 ksi
Schott F2HT Glass
Information Provided by SCHOTT North America, Inc.
Modulus of Elasticity 57.0 GPa
8270 ksi
Schott SF56A Glass
Information Provided by SCHOTT North America, Inc.