Mechanical Properties Metric English Comments
Modulus of Elasticity 51.0 GPa
7400 ksi
Schott Glass 8337B Borosilicate Glass
Borosilicate glass for sealing to Kovar metal and tungsten, highly UV-transmitting photomultiplier and UV detectors The heavy metal content for the elements lead, cadmium, mercury, and hexavalent ..
Modulus of Elasticity 51.0 GPa
7400 ksi
Corning 7070 Lithia Potash Borosilicate Crushed/Powdered Glass
Available in mesh sizes 4 through 325 and can be customized. Devitrifies before reaching a softening point. Used for sealing and other applications.Information provided by Corning Incorporated.