Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 5.86 - 22.1 GPa | 850 - 3200 ksi | Average value: 10.4 GPa Grade Count:21 |
Overview of materials for Polycarbonate, NCG Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, NCG Filled". Each property range of values reported is minimum and maximum values of appr.. |
|||
Modulus of Elasticity | 5.86 - 20.0 GPa | 850 - 2900 ksi | Average value: 11.6 GPa Grade Count:36 |
Overview of materials for Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled". Each property range of values reported is minimum.. |
|||
Modulus of Elasticity | 5.86 GPa | 850 ksi | ASTM D638 |
ITW Devcon Plastic Steel® Metal Repair (A), Dark Grey Information provided by ITW Devcon |
|||
Modulus of Elasticity | 5.86 GPa | 850 ksi | In Tension; ASTM D638 |
Devcon Plastic Steel® Liquid (B) Epoxy General Repair EpoxyComments: Steel-filled liquid epoxy can be cast over models for accurate detail reproduction when making holding fixtures, light-gauge forming dies and molds. Hardens in about a.. |
|||
Modulus of Elasticity | 5.86 GPa | 850 ksi | In Tension; ASTM D638 |
Devcon Plastic Steel® Putty (A) Epoxy General Repair EpoxyComments: The original metal-filled epoxy putty used for hundreds of routine maintenance, production and tooling applications. Bonds to most metal, concrete and some plastics. .. |
|||
Modulus of Elasticity | 5.86 GPa | 850 ksi | In Tension; ASTM D638 |
Devcon Wear Guard (Fine Load) Epoxy Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives. |
|||
Modulus of Elasticity | 5.86 GPa | 850 ksi | In Tension; ASTM D638 |
Devcon Wear Guard (High Temp) Epoxy Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives. |
|||
Modulus of Elasticity | 5.86 GPa | 850 ksi | In Tension; ASTM D638 |
Devcon Fastmeal™ Epoxy Precision Repair EpoxyComments: High-performance, alumina-filled epoxy putty for making fast, dependable emergency repair to leaks in pipes carrying ores, coal, cement, san and gravel. Cures in 5 m.. |
|||
Modulus of Elasticity | 5.86 GPa | 850 ksi | In Tension; ASTM D638 |
Devcon Wear Guard (High Load) Epoxy Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives. |
|||
Modulus of Elasticity | 5.86 - 18.0 GPa | 850 - 2610 ksi | Average value: 11.7 GPa Grade Count:17 |
Overview of materials for Nylon 46, Flame Retarded + Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Flame Retarded + Glass Fiber Reinforced". Each property range of values reported is minimum an.. |
|||
Modulus of Elasticity | 5.86 - 9.00 GPa | 850 - 1310 ksi | Average value: 8.07 GPa Grade Count:12 |
Overview of materials for Polyphenylene Ether, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 30% Glass Filled". Specific grades with glass content between 25% and 34% are inclu.. |