Polymer Property : Modulus of Elasticity = 48.2 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 48.2 GPa
6990 ksi
Parallel to pressing direction
Momentive Performance Materials HBC Hot-Pressed Boron Nitride
Hot-pressed BN is compacted at temperatures up to 2000°C and pressures up to 2000 psi to form a dense, strong engineering material that is easily machined. It is available in standard and custom..
Modulus of Elasticity 48.2 GPa
6990 ksi
Perpendicular to pressing direction
Momentive Performance Materials HBR Hot-Pressed Boron Nitride
Hot-pressed BN is compacted at temperatures up to 2000°C and pressures up to 2000 psi to form a dense, strong engineering material that is easily machined. It is available in standard and custom..