Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 44.1 GPa | 6400 ksi | |
Magnesium Elektron Elektron® 21 Magnesium Casting Alloy Fully heat treatable alloy for use up to 400°F. Excellent corrosion resistance and castability. Cast products possess a fine-grained microstructure and pressure tightness. Easily machined. Usual .. |