Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 400 GPa | 58000 ksi | |
Specialty Materials Boron Monofilament Exceptional compression strength. Specialty Materials' Chemical Vapor Deposition process uses fine tungsten wire for the substrate and boron trichloride gas as the boron source.Information prov.. |
|||
Modulus of Elasticity | 400 GPa | 58000 ksi | |
Sapco 99.9% Aluminum Oxide Information provided by Sapco. |
|||
Modulus of Elasticity | 400 GPa | 58000 ksi | |
Ceradyne CeraTrex™ 146-IS Silicon Carbide Features:high puritycorrosion resistancewear resistanceApplications:semiconductor componentssputtering targetsInformation provided by Ceradyne Company |