Polymer Property : Modulus of Elasticity = 375 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 375 GPa
54400 ksi
ASTM C848
CoorsTek SC-DSLP (SC-50) Liquid Phase Sintered Silicon Carbide
Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..