Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 372 GPa | 54000 ksi | ASTM-C848 |
CoorsTek ADS-995 99.5% Alumina Thin Film Applications: thin film substrates |
|||
Modulus of Elasticity | 372 GPa | 54000 ksi | ASTM-C848 |
CoorsTek ADS-996 99.6% Alumina Thin Film Applications: thin film substrates |
|||
Modulus of Elasticity | 372 GPa | 54000 ksi | ASTM-C848 |
CoorsTek Superstrate® 996 99.6% Alumina Thin Film Applications: thin film substrates |
|||
Modulus of Elasticity | 372 GPa | 54000 ksi | ASTM-C848 |
CoorsTek Superstrate® TPS 99.6% Alumina Thin Film Applications: thin film substrates |