Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Modulus of Elasticity = 36.5 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 36.5 - 40.0 GPa
5290 - 5800 ksi
Ceradyne Thermo-Sil® UHS Fused Silica
Fused Silica is an excellent thermal insulator with an extremely low coefficient of thermal expansion. It is excellent for thermal shock applications. The key characteristics of this material are:Hi..