Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 30.3 GPa | 4400 ksi | |
SGL Carbon Group EK 17 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Modulus of Elasticity | 30.3 GPa | 4400 ksi | |
SGL Carbon Group EK 3205 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Modulus of Elasticity | 30.3 GPa | 4400 ksi | |
SGL Carbon Group EK 3235 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Modulus of Elasticity | 30.3 GPa | 4400 ksi | X; ASTM D3039 |
Park Electrochemical Nelco® N4000-6 FC Multifunctional Epoxy Laminate and Prepreg The Nelco® N4000-6 FC is a high-Tg epoxy laminate and prepreg system that provides a wide range of performance versatility and ease of processing for demanding high-layer count applications.Key Fea.. |