Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 3.65 GPa | 529 ksi | ASTM D-638 |
Plaskolite Optix® CA - 75 HID General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Modulus of Elasticity | 3.65 GPa | 529 ksi | ASTM D-638 |
Plaskolite Optix® CA - 75 LL General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Modulus of Elasticity | 3.65 GPa | 529 ksi | ASTM D-638 |
Plaskolite Optix® CA - 75 OG General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Modulus of Elasticity | 3.65 GPa | 529 ksi | ASTM D-638 |
Plaskolite Optix® CA - 75 UVA General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Modulus of Elasticity | 3.65 GPa | 529 ksi | ASTM D-638 |
Plaskolite Optix® CA - 75 UVT General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Modulus of Elasticity | 3.65 GPa | 530 ksi | ASTM D-638 |
Plaskolite Optix® CA - 87 General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Modulus of Elasticity | 3.65 GPa | 529 ksi | ASTM D638 |
Plaskolite Optix® CA-86 Clear General Purpose Acrylic Resin General purpose acrylic resin, extrusion and injection molding gradeApplications: A general-purpose acrylic resin designed for high heat application. This resin offers the highest heat resistance a.. |
|||
Modulus of Elasticity | 3.65 GPa | 530 ksi | ASTM D-638 |
Plaskolite Optix® CP - 86 General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Modulus of Elasticity | 3.65 GPa | 529 ksi | ASTM D-638 |
Plaskolite West Optix® CA - 75 HID General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Modulus of Elasticity | 3.65 GPa | 529 ksi | ASTM D-638 |
Plaskolite West Optix® CA - 75 UVA General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Modulus of Elasticity | 3.65 GPa | 530 ksi | ASTM D-638 |
Plaskolite West Optix® CA - 87 General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Modulus of Elasticity | 3.65 GPa | 529 ksi | ASTM D638 |
Plaskolite West Optix® CA-86 Clear General Purpose Acrylic Resin General purpose acrylic resin, extrusion and injection molding gradeApplications: A general-purpose acrylic resin designed for high heat application. This resin offers the highest heat resistance a.. |
|||
Modulus of Elasticity | 3.65 GPa | 529 ksi | ASTM D-638 |
Plaskolite West Optix® CP - 75 HID General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Modulus of Elasticity | 3.65 GPa | 530 ksi | ASTM D-638 |
Plaskolite West Optix® CP - 86 General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Modulus of Elasticity | 3.65 GPa | 529 ksi | ASTM D-638 |
Plaskolite West Optix® CA - 75 LL General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Modulus of Elasticity | 3.65 GPa | 529 ksi | ASTM D-638 |
Plaskolite West Optix® CP - 75 UVA General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Modulus of Elasticity | 3.65 GPa | 530 ksi | ASTM D-638 |
Plaskolite West Optix® CP - 86 UVA General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Modulus of Elasticity | 3.65 GPa | 529 ksi | ASTM D-638 |
Plaskolite Optix® CP - 75 General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Modulus of Elasticity | 3.65 GPa | 529 ksi | ASTM D-638 |
Plaskolite Optix® CP - 75 HID General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Modulus of Elasticity | 3.65 GPa | 529 ksi | ASTM D-638 |
Plaskolite Optix® CP - 75 UVA General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Modulus of Elasticity | 3.65 GPa | 530 ksi | ASTM D-638 |
Plaskolite Optix® CP - 86 UVA General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Modulus of Elasticity | 3.65 GPa | 529 ksi | ASTM D-638 |
Plaskolite West Optix® CA - 75 OG General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Modulus of Elasticity | 3.65 GPa | 529 ksi | ASTM D-638 |
Plaskolite West Optix® CA - 75 UVT General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Modulus of Elasticity | 3.65 GPa | 529 ksi | ASTM D-638 |
Plaskolite West Optix® CP - 75 General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |