Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 3.50 GPa | 508 ksi | 50% RH |
Murtfeldt Murylat® Polyethylene Terephthalate Thanks to its extremely low absorption of moisture and low expansion coefficient, Murylat® is ideally suited for the processing of precision parts. Murylat® has an extremely high hardness grade an.. |
|||
Modulus of Elasticity | 3.50 - 24.1 GPa | 508 - 3500 ksi | Average value: 7.16 GPa Grade Count:21 |
Overview of materials for Polyphthalamide (PPA), Aramid Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Aramid Fiber". Each property range of values reported is minimum and maximum values of .. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | |
Lehmann & Voss LUVOCOM® 1106-8032/GY Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | |
Lehmann & Voss LUVOCOM® 19-7810 Polyamide 46, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Good friction and wear behaviour especially at increased temperatures.Emergency running propert.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | |
Lehmann & Voss LUVOCOM® 19-8073 Polyamide 46, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Good friction and wear behaviour especially at increased temperatures.Emergency running propert.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | |
Lehmann & Voss LUVOCOM® 19-8074 Polyamide 46, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Good friction and wear behaviour especially at increased temperatures.Emergency running propert.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | |
Lehmann & Voss LUVOCOM® 6-8512 Polyamide 12, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Especially suitable at dynamic.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | Sample Type 1B, 50 mm/min; ISO 527-1/2:1993 |
Global EPP PET SL PET + Solid Lubricant PET is an unreinforced, semi-crystalline thermoplastic polyester, demonstrating dimensional stability similar to acetal, combined with the comparable wear resistance of nylon. Heavily loaded mechani.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | |
Lehmann & Voss LUVOCOM® 1105/GY7993 PEEK, unreinforced Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | |
Lehmann & Voss LUVOCOM® 1105-1330 PEEK, with PTFE Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | |
Lehmann & Voss LUVOCOM® 1106-8154/GY Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | ISO 527-2 |
Tisan TISLAMID® 66 15% Mineral Filled Flame Retardant (V0). Heat Stabilized Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | TD; ExxonMobil Method |
ExxonMobil Bicor™ 15MB440 OPP Film Product Description: Bicor 15MB440 is a biaxially oriented transparent polypropylene film designed to be the outside web of a laminate.Availability: Arica & Middle East, Asia Pacific, Europe, Latin .. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | TD; ExxonMobil Method |
ExxonMobil Bicor™ 20MB400 OPP Film Product Description: Bicor 20MB400 is a one side treated, sealable coextruded OPP film. It is designed for use in laminations.Availability: Africa & Middle East, Asia Pacific and EuropeKey Features:.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | TD; ExxonMobil Method |
ExxonMobil Bicor™ 30MB666 OPP Film Product Description: A biaxially oriented transparent polypropylene film, acrylic coated two sides. It provides outstanding performance on all packaging machines.Availability: Africa & Middle East, .. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | TD; ExxonMobil Method |
ExxonMobil Bicor™ 30MBR666 OPP Film Product Description: Bicor 30MBR is a biaxially oriented transparent polypropylene film coated with humidity resistant acrylic on both sides. This film is designed to wrap products with a high moist.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | TD; ExxonMobil Method |
ExxonMobil Bicor™ 35MB666 OPP Film Product Description: A is a biaxially oriented transparent polypropylene film, acrylic coated tow sides. It provides outstanding performance on all packaging machines.Availability: Africa & Middle E.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | TD; ExxonMobil Method |
ExxonMobil Bicor™ 40MB668 OPP Film Product Description: A high speed transparent biaxially oriented polypropylene film, coated one side acrylic, one side very low temperature seal (VLTS) coating. VLTS coating provides excellent perfo.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | TD; ExxonMobil Method |
ExxonMobil Bicor™ 42MB777 OPP Film Product Description: A high gas barrier, biaxially oriented transparent PP film, coated one side PVdC, one side acrylic, This film provides outstanding performance on all packaging machines.Availabi.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | TD; ExxonMobil Method |
ExxonMobil Label-Lyte™ 17LL222 OPP Film Product Description: An uncoated biaxially oriented, transparent polypropylene film designed for overlamination in labeling applications where high gloss and high transparency are required.Availabil.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | TD; ExxonMobil Method |
ExxonMobil Label-Lyte™ 30LL666 OPP Film Product Description: A transparent, high gloss, two side acrylic coated BOPP film for reel-fed wrap-around labeling applications.Availability: Africa & Middle East, Asia Pacific and EuropeKey Featur.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | TD; ExxonMobil Method |
ExxonMobil Label-Lyte™ 50LGT702 OPP Film Product Description: A transparent biaxially oriented polypropylene film coated one side resistant coating and one side with a specially formulated acrylic coating. This film is designed for cut and.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | TD; ExxonMobil Method |
ExxonMobil Label-Lyte™ 50LL210 OPP Film Product Description: An uncoated biaxially oriented, transparent polypropylene film for Pressure Sensitive labeling applications.Availability: Africa & Middle East, Asia Pacific and EuropeKey Featur.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | TD; ExxonMobil Method |
ExxonMobil Label-Lyte™ 50LL539 OPP Film Product Description: A clear, two-side coated, polypropylene label face stock designed for demanding pressure sensitive applications where outstanding ink adhesion and adhesive anchorage are require.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | TD; ExxonMobil Method |
ExxonMobil Label-Lyte™ 50ML580 OPP Film Product Description: A metalized, surface printable OPP film designed for pressure sensitive applications where high-sheen metalized appearance and high-speed press performance are desired. The prop.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | TD; ExxonMobil Method |
ExxonMobil Bicor™ 17MB400 OPP Film Product Description: Bicor 17MB400 is one side treated, sealable coextruded OPP film. It is designed for use in laminations.Availability: Africa & Middle East, Asia Pacific and EuropeKey Features:Ou.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | Conditioned; ISO 178 |
Addiplast Addinyl A2 V15 Nylon 66, 15% Glass Filled Glass fiber reinforced, high strengthInformation provided by Addiplast. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | Conditioned; ISO 178 |
Addiplast Addinyl A2 ZV15 Nylon 66, 15% Glass Filled Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | ISO 527-1/-2 |
BASF Ultramid® B3EG3 BK 00564 15% Glass Filled PA6 (Conditioned) Description: 15% glass-fiber reinforced injection-molding grade with enhanced impact resistance, for example, for vehicle mirror housings as well as for the wheels of mountain bikes.Information prov.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | Conditioned; ISO 178 |
Addiplast Addinyl B2H M30 Flame Retardant Nylon 6, 30% Mineral Filled Flame retardant, 30% mineral filled, with halogensInformation provided by Addiplast. |