Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 3.31 GPa | 480 ksi | ASTM D638 |
Ineos Nova 2580 General Purpose Crystal Polystyrene
(discontinued **) High speed molding, Improved crack resistanceApplications: Cutlery, Consumer electronicsExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the physical and optic.. |
|||
Modulus of Elasticity | 3.31 GPa | 480 ksi | ASTM D638 |
Ineos Nova 2510 General Purpose Crystal Polystyrene
(discontinued **) High speed molding, Improved crack resistance, USP Class VIApplications: Cutlery, Light louvers, RazorsExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the phy.. |
|||
Modulus of Elasticity | 3.31 GPa | 480 ksi | ASTM D638 |
Ineos Nova 2511 General Purpose Crystal Polystyrene
(discontinued **) High speed molding, Improved crack resistance, USP Class VIApplications: Cutlery, Light louvers, RazorsExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the phy.. |
|||
Modulus of Elasticity | 3.31 GPa | 480 ksi | 50 mm/min; ASTM D638 |
LG Chemical 95HC SAN Resin Heat and chemical resistance, Good mechanical properties, Excellent processability, Superior transparency, Good dimensional stability, Applications include make-up cases and other products requiring.. |