Polymer Property : Modulus of Elasticity = 294 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 294 GPa
42600 ksi
Plansee Chromium, Cr; Sintered
Characteristics:High corrosion resistanceHigh wear resistanceBeautiful opticsLower melting point than other refractory metalsVery high vapor pressureLower density than other refractory metalsPossess..