Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 276 GPa | 40000 ksi | |
Hogen HM1000 Tungsten-Based Metal Mil Spec T-21014D Class 1; ASTM B-777-99 Class 1; SAE Aero Material Spec (AMS) 7725C; AMS T-21014 Class 1. Nil magnetic properties.Manufactured by powder metallurgy methods. The tungsten base offe.. |
|||
Modulus of Elasticity | 276 GPa | 40000 ksi | |
Mi-Tech Metals HD17 Tungsten-Based Metal Mil Spec T-21014D Class 1; ASTM B-777-99 Class 1; ASTM B-777-07 Class 1; SAE Aero Material Spec (AMS) 7725C; AMS T-21014 Class 1. Nil magnetic properties.Manufactured by powder metallurgy methods. .. |
|||
Modulus of Elasticity | 276 GPa | 40000 ksi | |
Mi-Tech Metals HD17BB Tungsten-Based Metal ASTM B-777-07 Class 1; Slightly Magnetic (HD17 is non-magnetic).Manufactured by powder metallurgy methods. The tungsten base offers high thermal conductivity and a low CTE which combine to resist t.. |
|||
Modulus of Elasticity | 276 GPa | 40000 ksi | Tensile modulus calculated at secant 6000-1000 |
Hexcel® IM4 Carbon Fiber (12,000 Filaments) Weight/length = 0.723 g/m.Information provided by Hexcel Corporation. Values are typical average lot properties.Continuous fiber can be combined with virtually all thermoset and thermoplastic resin.. |
|||
Modulus of Elasticity | 276 GPa | 40000 ksi | Tensile modulus calculated at secant 6000-1000 |
Hexcel® IM6 Carbon Fiber (12,000 Filaments) Weight/length = 0.446 g/m.Information provided by Hexcel Corporation. Values are typical average lot properties.Continuous fiber can be combined with virtually all thermoset and thermoplastic resin.. |
|||
Modulus of Elasticity | 276 GPa | 40000 ksi | Tensile modulus calculated at secant 6000-1000 |
Hexcel® IM7 Carbon Fiber (12,000 Filaments) Weight/length = 0.446 g/m.Information provided by Hexcel Corporation. Values are typical average lot properties.Continuous fiber can be combined with virtually all thermoset and thermoplastic resin.. |
|||
Modulus of Elasticity | 276 GPa | 40000 ksi | Tensile modulus calculated at secant 6000-1000 |
Hexcel® IM7 Carbon Fiber (6000 Filaments) Weight/length = 0.223 g/m.Information provided by Hexcel Corporation. Values are typical average lot properties.Continuous fiber can be combined with virtually all thermoset and thermoplastic resin.. |
|||
Modulus of Elasticity | 276 GPa | 40000 ksi | Tensile modulus calculated at secant 6000-1000 |
Hexcel® IM9 Carbon Fiber (12,000 Filaments) Weight/length = 0.331 g/m.Information provided by Hexcel Corporation. Values are typical average lot properties.Continuous fiber can be combined with virtually all thermoset and thermoplastic resin.. |
|||
Modulus of Elasticity | 276 GPa | 40000 ksi | ASTM C848 |
CoorsTek AD-90 Alumina (nom. 90% Al2O3) Thermal Shock Delta Tc = 250°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Modulus of Elasticity | 276 GPa | 40000 ksi | At 55° to rolling direction |
AK Steel TRAN-COR® H-0 CARLITE® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Modulus of Elasticity | 276 GPa | 40000 ksi | At 55° to rolling direction |
AK Steel TRAN-COR® H-1 CARLITE® DR® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Modulus of Elasticity | 276 GPa | 40000 ksi | At 55° to rolling direction |
AK Steel TRAN-COR® H-1 CARLITE® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Modulus of Elasticity | 276 GPa | 40000 ksi | At 55° to rolling direction |
AK Steel TRAN-COR® H-2 CARLITE® DR® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Modulus of Elasticity | 276 GPa | 40000 ksi | At 55° to rolling direction |
AK Steel TRAN-COR® H-2 CARLITE® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Modulus of Elasticity | 276 GPa | 40000 ksi | At 55° to rolling direction |
AK Steel TRAN-COR® H-0 CARLITE® DR® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |