Mechanical Properties Metric English Comments
Modulus of Elasticity 26.5 GPa
3840 ksi
ASMT D638
Toyobo TS101 PPS, Glass Fiber/Mineral Reinforced
Key Feature: High dimensional stabilityHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology developed by Toyobo. Excellent..