Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 241 GPa | 35000 ksi | |
Specialty Materials Hy-Bor Boron/Graphite Hybrid Prepreg Tape Boron & Graphite prepreg. Combining Specialty Materials' boron fiber with graphite prepreg, Hy-Bor® is a high-performance material with exceptional properties. Available with 4.0 and 5.6 mil.. |
|||
Modulus of Elasticity | 241 GPa | 35000 ksi | Tensile modulus calculated at secant 6000-1000 |
Hexcel® AS4D Carbon Fiber (12,000 Filaments) Weight/length = 0.765 g/m.Information provided by Hexcel Corporation. Values are typical average lot properties.Continuous fiber can be combined with virtually all thermoset and thermoplastic resin.. |
|||
Modulus of Elasticity | 241 GPa | 35000 ksi | In Tension |
Cytec Thornel® T-650/35 3K Carbon Fiber, Polyacrylonitrile (PAN) Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous length, high strength, high modulus fiber made from a polyacrylonitrile precursor. The fiber surface has been treated t.. |
|||
Modulus of Elasticity | 241 GPa | 35000 ksi | In Tension |
Cytec Thornel® T-650/35 6K Carbon Fiber, Polyacrylonitrile (PAN) Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous length, high strength, high modulus fiber made from a polyacrylonitrile precursor. The fiber surface has been treated t.. |
|||
Modulus of Elasticity | 241 GPa | 35000 ksi | |
CMW® THERMKON® 70M Molybdenum Copper parts For matching CTE of semiconductor substrates while allowing high thermal transfer.Information provided by CMW Inc. |
|||
Modulus of Elasticity | 241 GPa | 35000 ksi | |
CMW® THERMKON® 76 Tungsten Copper parts For matching CTE of semiconductor substrates while allowing high thermal transfer.Information provided by CMW Inc. |
|||
Modulus of Elasticity | 241 GPa | 35000 ksi | At 45° to rolling direction |
AK Steel TRAN-COR® H-0 CARLITE® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Modulus of Elasticity | 241 GPa | 35000 ksi | At 45° to rolling direction |
AK Steel TRAN-COR® H-1 CARLITE® DR® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Modulus of Elasticity | 241 GPa | 35000 ksi | At 45° to rolling direction |
AK Steel TRAN-COR® H-1 CARLITE® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Modulus of Elasticity | 241 GPa | 35000 ksi | At 45° to rolling direction |
AK Steel TRAN-COR® H-2 CARLITE® DR® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Modulus of Elasticity | 241 GPa | 35000 ksi | At 45° to rolling direction |
AK Steel TRAN-COR® H-2 CARLITE® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Modulus of Elasticity | 241 GPa | 35000 ksi | At 45° to rolling direction |
AK Steel TRAN-COR® H-0 CARLITE® DR® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |