Polymer Property : Modulus of Elasticity = 240 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 240 GPa
34800 ksi
Kennametal Stellite Delcrome® 93
Information provided by Deloro Stellite, Inc. Typical data, not guaranteed as a maximum or minimum. Highly alloyed white cast iron, abrasion resistant. Carbides in a martensitic matrix offer high..
Modulus of Elasticity 240 GPa
34800 ksi
H.C. Starck WCu 75/25 Tungsten-Copper Composite Material
Description of Product: Tungsten-copper composite materials are produced by copper infiltration of porous sintered tungsten. They are available with different copper contents (10 - 30 %). A therm..
Modulus of Elasticity 240 GPa
34800 ksi
ASTM D3379-94
SGL Carbon Group SIGRAFIL C® C30 S003 GLY Staple Carbon Fiber, Glycerine Sizing
In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making..
Modulus of Elasticity 240 GPa
34800 ksi
ASTM D3379-95
SGL Carbon Group SIGRAFIL C® C30 S006 GLY Staple Carbon Fiber, Glycerine Sizing
In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making..
Modulus of Elasticity 240 GPa
34800 ksi
ASTM D3379-96
SGL Carbon Group SIGRAFIL C® C30 S009 GLY Staple Carbon Fiber, Glycerine Sizing
In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making..
Modulus of Elasticity 240 GPa
34800 ksi
ASTM D3379-97
SGL Carbon Group SIGRAFIL C® C30 S012 GLY Staple Carbon Fiber, Glycerine Sizing
In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making..
Modulus of Elasticity 240 GPa
34800 ksi
ASTM D3379-77
SGL Carbon Group SIGRAFIL C® C30 T050 EPY Continuous Tow Carbon Fiber with 50k filaments, Epoxy Sizing
SIGRAFIL C as continuous tow is ideal for waving, prepregging, filament winding, Carbon Fiber Reinforced Plastics (CFRP) components, advanced composites, multi-axial production, unidirectional tapes..
Modulus of Elasticity 240 GPa
34800 ksi
ASTM D3379-78
SGL Carbon Group SIGRAFIL C® C30 T400 EPY Continuous Tow Carbon Fiber with 400k filaments, Epoxy Sizing
SIGRAFIL C as continuous tow is ideal for waving, prepregging, filament winding, Carbon Fiber Reinforced Plastics (CFRP) components, advanced composites, multi-axial production, unidirectional tapes..
Modulus of Elasticity 240 GPa
34800 ksi
Bohler-Uddeholm BÖHLER S590 MICROCLEAN® High Speed Steel
Description: High speed steel produced by powder-metallurgy methods with highest red hardness, compressive strength and wear resistance. The PM technology imparts to the material also excellent toug..
Modulus of Elasticity 240 GPa
34800 ksi
(hardened to 58 HRC)
Bohler-Uddeholm UDDEHOLM ELMAX® Powder Metallurgy Stainless Mold Steel
High chromium-vanadium-molybdenum alloyed steelA through-hardening corrosion resistant mold steel made by powder metallurgy processing techniques. The high wear resistance makes ELMAX® suitable for..
Modulus of Elasticity 240 GPa
34800 ksi
Assab Steels ASP 30 Cold Work Steel
ASP 30 is a W-Mo-v-Co alloyed PM high speed steel characterized by:High wear resistanceHigh compressive strength at high hardnessGood through hardening propertiesGood toughnessGood dimensional stabi..