Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 234 GPa | 33900 ksi | |
Kennametal Stellite Stellite® 19 Can be machined with carbide tipped tools, but when hardness exceeds Rc55 it is best to grind. Applications include cutting tools, bearing races, guide rolls, and nozzle discs. Excellent resistance .. |
|||
Modulus of Elasticity | 234 GPa | 34000 ksi | |
Crucible Compaction Metals CPM® VIM CRU® 20® CPM® VIM CRU® 20® is a vacuum induction melted, cobalt-free super high speed steel manufactured by the Crucible Particle Metallurgy (CPM®) process. VIM CRU processing is designed to meet the cle.. |
|||
Modulus of Elasticity | 234 GPa | 33900 ksi | |
CMW® THERMKON® 83 Tungsten Copper parts For matching CTE of semiconductor substrates while allowing high thermal transfer.Information provided by CMW Inc. |
|||
Modulus of Elasticity | 234 GPa | 34000 ksi | (hardened and tempered) |
Bohler-Uddeholm UDDEHOLM VANADIS 30 AISI M2 + Co SUPERCLEAN 3 Powder Metallurgical Cold Work Tool Steel Uddeholm Vanadis 30 is a Co high alloyed powder metallurgy high speed steel corresponding to AISI M3:2 + Co. The high compressive strength, 67 HRC, and good abrasive wear resistance makes Uddeholm V.. |
|||
Modulus of Elasticity | 234 GPa | 33900 ksi | |
Assab Steels VANADIS 10 Cold Work Steel VANADIS 4 is a chromium-molybdenum-vanadium alloyed steel which is characterized by:Extremely high abrasive wear resistanceHigh compressive strengthVery good through-hardening propertiesGood toughne.. |