Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 21.0 GPa | 3050 ksi | DIN 53 457 |
Albis Plastics Tedur® L V 9113-2 PPS, 60% Glass Fiber
(discontinued **) Glass Fiber Grade with Highest Mechanical Strength and Stiffness. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Housings for Shock Absorbers and Spring ElementsProce.. |
|||
Modulus of Elasticity | 21.0 GPa | 3050 ksi | |
Lehmann & Voss LUVOCOM® 1105-8529 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Modulus of Elasticity | 21.0 GPa | 3050 ksi | |
Lehmann & Voss LUVOCOM® 1301-8066 PPS, linear, with carbon fiber, lubricant modified, high viscosity Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
Modulus of Elasticity | 21.0 GPa | 3050 ksi | |
Lehmann & Voss LUVOCOM® 1-7390 Polyamide 66, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Modulus of Elasticity | 21.0 GPa | 3050 ksi | |
Lehmann & Voss LUVOCOM® 1-7532 Polyamide 66, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Modulus of Elasticity | 21.0 GPa | 3050 ksi | |
Lehmann & Voss LUVOCOM® 20-7343 Polyphthalamide, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an.. |
|||
Modulus of Elasticity | 21.0 GPa | 3050 ksi | |
Indium Corp. Indalloy 141 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Modulus of Elasticity | 21.0 GPa | 3050 ksi | |
Lehmann & Voss LUVOCOM® 1105/XCF/20 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Modulus of Elasticity | 21.0 GPa | 3050 ksi | |
Lehmann & Voss LUVOCOM® 1106-8133 Polyether imide, with carbon fiber, easy flowing Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.High dimensionally stable precision parts.Electrical.. |
|||
Modulus of Elasticity | 21.0 GPa | 3050 ksi | |
Lehmann & Voss LUVOCOM® 1301-7629/EG PPS, linear, with carbon fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
Modulus of Elasticity | 21.0 GPa | 3050 ksi | |
Lehmann & Voss LUVOCOM® 1850-7487 PBT, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Modulus of Elasticity | 21.0 GPa | 3050 ksi | |
Lehmann & Voss LUVOCOM® 1/XCF/25 Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Modulus of Elasticity | 21.0 GPa | 3050 ksi | |
Lehmann & Voss LUVOCOM® 1301/CF/10/GF/20/GK/20/BK100 PPS, linear, with carbon fiber, glass fiber and micro glass spheres Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |