Polymer Property : Modulus of Elasticity = 2.77 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 2.77 - 16.5 GPa

@Temperature -40.0 - 250 °C
402 - 2390 ksi

@Temperature -40.0 - 482 °F
Average value: 7.45 GPa Grade Count:1
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max..
Modulus of Elasticity 2.77 - 16.5 GPa

@Thickness 1.60 - 3.17 mm
402 - 2390 ksi

@Thickness 0.0630 - 0.125 in
Average value: 7.45 GPa Grade Count:1
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled