Polymer Property : Modulus of Elasticity = 2.55 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 2.55 - 26.7 GPa

@Temperature 60.0 - 150 °C
370 - 3870 ksi

@Temperature 140 - 302 °F
Average value: 20.0 GPa Grade Count:4
Overview of materials for Polyetheretherketone, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu..
Modulus of Elasticity 2.55 GPa
370 ksi
ASTM D638
Ineos Nova 4211 Medium Impact Polystyrene  (discontinued **)
Excellent balance of properties, USP Class VIApplications: Consumer electronics, Injection molding applicationsProperties were determined on injection molded specimens at 23°C and 50% R.H. unless o..
Modulus of Elasticity 2.55 GPa
370 ksi
DIN 53457
Ineos Nova S-5100 High Impact Compact Polystyrene  (discontinued **)
All mechanical properties measured under standard conditions 50% RH and 23°C.Information provided by NOVA Chemicals.INEOS NOVA began October 1 2007 as an expansion of the 50:50 joint venture betwee..
Modulus of Elasticity 2.55 - 2.82 GPa
370 - 409 ksi
Average value: 2.70 GPa Grade Count:8
Overview of materials for PVC, Sheet Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Sheet Grade". Each property range of values reported is minimum and maximum values of appropriate M..
Modulus of Elasticity 2.55 GPa
370 ksi
Secant; ASTM D5026
Specialty Coating Systems Parylene HT® Poly (P-Xylylene) Coating
Parylene HT is a polymer of para-xylylene with the alpha hydrogen atoms of the N dimer replaced with fluorine. This variant of Parylene is useful in high temperature applications (short term up to 4..
Modulus of Elasticity 2.55 - 2.93 GPa

@Temperature 22.8 °C
370 - 425 ksi

@Temperature 73.0 °F
Ensinger TECAST VEKTON™ 6PB Nylon 6 (PA6)
TECAST VEKTON™ 6PB cushion pads are used to dampen the shock load on the anvil of a pile hammer. Specially formulated from an impact-modified type 6 nylon, they combine the excellent strength of n..
Modulus of Elasticity 2.55 - 7.00 GPa
370 - 1020 ksi
Average value: 5.73 GPa Grade Count:12
Overview of materials for Polysulfone, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are inc..
Modulus of Elasticity 2.55 GPa
370 ksi
ASTM D638
GEHR Plastics Noryl PPO  (discontinued **)
PPO belongs to the group of the amorphous materials and can be used in temperatures ranging from -58 °F to +302 °F. PPO exhibits a high impact strength and a very high dimensional stability. The e..