Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 2.40 - 3.40 GPa @Temperature 60.0 - 120 °C |
348 - 493 ksi @Temperature 140 - 248 °F |
Average value: 2.87 GPa Grade Count:1 |
Overview of materials for Polyphenylene Ether, 10% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 10% Glass Filled". Specific grades with glass content between 5% and 14% are includ.. |
|||
Modulus of Elasticity | 2.40 GPa | 348 ksi | DIN 53457 |
Ineos Nova S-2200 Medium Impact Compact Polystyrene
(discontinued **) Medium impact easy flowing polystyrene, designed for injection molding applications with short cycle times and for complicated technical parts. The product has a high stiffness and an excellent the.. |
|||
Modulus of Elasticity | 2.40 - 8.50 GPa | 348 - 1230 ksi | Average value: 4.67 GPa Grade Count:29 |
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar.. |
|||
Modulus of Elasticity | 2.40 GPa | 348 ksi | Youngs Modulus, ASTM D638, 10%/min. |
EVALCA EVAL® LC-H101BD Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 38 mol % Ethylene.Data provided by EVALCA. Applications: Blown film. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produced as a part of th.. |
|||
Modulus of Elasticity | 2.40 GPa | 348 ksi | Youngs Modulus, ASTM D638, 10%/min. |
EVALCA EVAL® K102 Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 38 mol % Ethylene.Data provided by EVALCA. Applications: Solid phase pressure forming. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produc.. |
|||
Modulus of Elasticity | 2.40 GPa | 348 ksi | Youngs Modulus, ASTM D638, 10%/min. |
EVALCA EVAL® G110 Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 48 mol % Ethylene.Data provided by EVALCA. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produced as a part of the Kuraray product line. |
|||
Modulus of Elasticity | 2.40 GPa | 348 ksi | ISO 527 |
Chevron Phillips Xtel® XE5300NA Polyphenylene Sulfide Alloy
(discontinued **) Xtel® XE5300NA is a high performance extrusion grade PPS based alloy developed to provide excellent mechanical strength, elongation and chemical resistance.Information provided by Chevron Phillips |
|||
Modulus of Elasticity | 2.40 GPa | 348 ksi | |
Lehmann & Voss LUVOCOM® 50/TF/15/BK7284 Polycarbonate, with PTFE, easy flowing Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper.. |
|||
Modulus of Elasticity | 2.40 GPa | 348 ksi | |
Lehmann & Voss LUVOCOM® 50/TF/15/GY77 Polycarbonate, with PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper.. |
|||
Modulus of Elasticity | 2.40 GPa | 348 ksi | ISO 527 |
GEHR Plastics PC Polycarbonate Polycarbonate shows a high rigidity and an extreme impact strength. Also it has a high glass transition temperature and temperature resistance. The operating temperature ranges from -60°C to appr.. |
|||
Modulus of Elasticity | 2.40 GPa | 348 ksi | |
Lehmann & Voss LUVOCOM® 1850/PL/15/BK PBT, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Parts for electric and electro.. |
|||
Modulus of Elasticity | 2.40 GPa | 348 ksi | |
Lehmann & Voss LUVOCOM® NSB 90 BK Polyamide 66, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Modulus of Elasticity | 2.40 GPa | 348 ksi | |
Lehmann & Voss LUVOCOM® PA66/TF/40 Polyamide 66, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Modulus of Elasticity | 2.40 GPa | 348 ksi | ISO 527-2 |
Tisan TISAKRIL® UNR ABS TISAKRIL has a wide area of application in automotive, electronics, computer, construction, and furniture industries. General Specifications include: High surface luminosityEasy processabilityDimens.. |
|||
Modulus of Elasticity | 2.40 GPa | 348 ksi | ISO 527-2 |
Tisan TISLAMID® 66 UNR Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Modulus of Elasticity | 2.40 GPa | 348 ksi | ISO 527-2 |
Tisan TISOPLEN® 15% Mineral Filled Flame Retardant (V0). Heat Stabilized Copolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Modulus of Elasticity | 2.40 GPa | 348 ksi | Conditioned; ISO 178 |
Addiplast Addilene H 590 RM20F Flame Retardant Polypropylene, 20% Mineral Filled Flame retardant, mineral filled, with halogens, impact resistantInformation provided by Addiplast. |
|||
Modulus of Elasticity | 2.40 GPa | 348 ksi | Conditioned; ISO 178 |
Addiplast Addilene J 490 M20S Flame Retardant Polypropylene, 20% Mineral Filled Flame retardant, mineral filled, with halogensInformation provided by Addiplast. |
|||
Modulus of Elasticity | 2.40 GPa | 348 ksi | Conditioned; ISO 178 |
Addiplast Addinyl B2H G30 Flame Retardant Nylon 6, 30% Glass Bead Flame retardant, 30% glass bead filled, with halogensInformation provided by Addiplast. |
|||
Modulus of Elasticity | 2.40 GPa | 348 ksi | ISO 527-2 |
BASF Ultraform® N2520 L POM Description: Is a POM, product having reduced electric surface resistance.Information provided by BASF |
|||
Modulus of Elasticity | 2.40 GPa | 348 ksi | ISO 527-1/-2 |
BASF Ultramid® S3K Balance PA 610 (Dry) Description: BASF supplies polyamide 610 for processing by injection molding under the trade name Ultramid® Balance which is produced by polycondensation of hexamethylene diamine and sebacic acid. .. |
|||
Modulus of Elasticity | 2.40 GPa | 348 ksi | 1 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 1012 PVDF Homopolymer
(discontinued **) Key features of this grade: High Viscosity, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-c.. |
|||
Modulus of Elasticity | 2.40 GPa | 348 ksi | 1% Secant; ASTM D638 |
Ensinger ENSIKEM® PVDF (Polyvinylidene Fluoride) - Extruded Products
(discontinued **) Polyvinylidene fluoride, or PVDF, is a fluorinated thermoplastic resin that has outstanding resistance to most mineral and organic acids, aliphatic and aromatic hydrocarbons, alcohols, halogenated s.. |
|||
Modulus of Elasticity | 2.40 GPa | 348 ksi | ISO 527-2 |
BASF Ultradur B 4520 PBT Ultradur B4520 is a medium viscosity, rapidly freezing injection molding grade. |
|||
Modulus of Elasticity | 2.40 GPa | 348 ksi | ISO 527-2 |
BASF Ultradur B 6550 PBT Ultradur B 6550 is a high viscosity PBT extrusion grade.Applications; Used for loose buffer tubes for optical fibers, semi-finished products fro machining, profiles and pipes. |
|||
Modulus of Elasticity | 2.40 - 36.6 GPa | 348 - 5300 ksi | Average value: 14.3 GPa Grade Count:30 |
Overview of materials for Polyethersulfone, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximu.. |
|||
Modulus of Elasticity | 2.40 - 12.3 GPa | 348 - 1780 ksi | Average value: 4.64 GPa Grade Count:45 |
Overview of materials for Polypropylene, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum .. |