Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 2.35 GPa | 341 ksi | ISO 527-2 |
Tisan TISOPLEN® 10% Talc Filled Heat Stabilized Homopolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Modulus of Elasticity | 2.35 GPa | 341 ksi | ISO 527-2 |
Tisan TISOPLEN® 40% Calcite Filled Heat Stabilized Copolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Modulus of Elasticity | 2.35 GPa | 341 ksi | ISO 527-2 |
Tisan TISOPLEN® 20% Talc Filled Heat Stabilized Homopolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Modulus of Elasticity | 2.35 GPa | 341 ksi | DIN 53457 |
Ineos Nova S-3207 Medium Impact Compact Polystyrene
(discontinued **) High flow medium impact polystyrene, designed of injection molding of low friction household goods, packaging and toys. It combines low friction properties with excellent (ultrasonic) weldability.A.. |