Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 2.28 GPa | 331 ksi | ASTM D638 |
PTS Trilac® ABS-RC3000 Recycled Black ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Modulus of Elasticity | 2.28 - 15.0 GPa | 331 - 2180 ksi | Average value: 9.02 GPa Grade Count:8 |
Overview of materials for PET + PBT Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "PET + PBT Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Modulus of Elasticity | 2.28 GPa | 331 ksi | 0.2 in/min; ASTM D638 |
Ineos Nova Zylar® 220 High Performance Styrenic, Acrylic Copolymer
(discontinued **) Excellent moldability, High clarity, Extended toughness and elongation, meets USP XXI specification for Class VI Plastics, Property retention after gamma irradiationApplications: Display, medical de.. |
|||
Modulus of Elasticity | 2.28 - 22.4 GPa | 331 - 3250 ksi | Average value: 10.4 GPa Grade Count:10 |
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Black Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Black Filled". Each property range of values reported is minimu.. |