Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | >= 2.25 GPa | >= 326 ksi | ISO 527/ASTM D638 |
Quadrant EPP Monocast® MC 904P Nylon for Pile Driver Pads (ASTM Product Data Sheet) Pile driver pads are used to prevent damage to the pile and the piling hammer. Fillers are usually made of hardwood - Azobe, for example. The disadvantage of Azobe is the 30-40% energy loss and it.. |
|||
Modulus of Elasticity | 2.25 - 3.50 GPa | 327 - 508 ksi | Average value: 3.02 GPa Grade Count:53 |
Overview of materials for Polystyrene, Transparent Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Transparent Grade". Each property range of values reported is minimum and maximum values of.. |
|||
Modulus of Elasticity | 2.25 GPa | 326 ksi | DIN 53457 |
Ineos Nova S-3222 Medium Impact Compact Polystyrene
(discontinued **) All mechanical properties measured under standard conditions 50% RH and 23°C.Information provided by NOVA Chemicals.INEOS NOVA began October 1 2007 as an expansion of the 50:50 joint venture betwee.. |
|||
Modulus of Elasticity | 2.25 - 10.0 GPa @Temperature 60.0 - 160 °C |
326 - 1450 ksi @Temperature 140 - 320 °F |
Average value: 5.59 GPa Grade Count:7 |
Overview of materials for Polyethersulfone (PES) This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Modulus of Elasticity | 2.25 - 15.0 GPa | 326 - 2180 ksi | Average value: 6.31 GPa Grade Count:143 |
Overview of materials for Polypropylene with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are i.. |