Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 180 GPa @Temperature 300 °C |
26100 ksi @Temperature 572 °F |
|
Outokumpu SAF 2304® Duplex Stainless Steel Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone.. |
|||
Modulus of Elasticity | 180 GPa @Temperature 300 °C |
26100 ksi @Temperature 572 °F |
|
Outokumpu SAF 2507® Duplex Stainless Steel Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone.. |
|||
Modulus of Elasticity | 180 GPa @Temperature 480 °C |
26100 ksi @Temperature 896 °F |
|
Haynes HR-160® alloy, annealed plate Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Modulus of Elasticity | 180 GPa @Temperature 480 °C |
26100 ksi @Temperature 896 °F |
|
Haynes HR-160® alloy, hot rolled and solution annealed plate Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Modulus of Elasticity | 180 GPa @Temperature 480 °C |
26100 ksi @Temperature 896 °F |
|
Haynes HR-160® alloy, plate, aged 1000 hours at 871°C (1600°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Modulus of Elasticity | 180 GPa @Temperature 480 °C |
26100 ksi @Temperature 896 °F |
|
Haynes HR-160® alloy, plate, aged 4000 hours at 760°C (1400°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Modulus of Elasticity | 180 - 193 GPa | 26100 - 28000 ksi | |
Materion Beryllium Nickel M220C Information supplied by Brush Wellman Engineered Materials.Brush M220C is characterized by high levels of strength, hardness, and thermal conductivity combined with excellent resistance to wear, cor.. |
|||
Modulus of Elasticity | 180 GPa @Temperature 480 °C |
26100 ksi @Temperature 896 °F |
|
Haynes HR-160® alloy plate, aged 8000 hours at 649°C (1200°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Modulus of Elasticity | 180 GPa @Temperature 399 °C |
26100 ksi @Temperature 750 °F |
hardened to 62 HRC |
Bohler-Uddeholm AISI D2 Cold Work Tool Steel AISI D2 is a high-carbon, high-chromium tool steel alloyed with molybdenum and vanadiumAISI AD2 is characterized by: High wear resistance High compressive strength Good through-hardening properties.. |
|||
Modulus of Elasticity | 180 GPa @Temperature 399 °C |
26100 ksi @Temperature 750 °F |
hardened to 52 HRC |
Bohler-Uddeholm POLMAX® 420 Modified - Stainless Mold Steel Polmax is an excellent choice for extreme surface finish requirements. This high performance grade achieves surface finishes that go well beyond conventional tool steels. Polmax is specifically eng.. |
|||
Modulus of Elasticity | 180 GPa @Temperature 399 °C |
26100 ksi @Temperature 750 °F |
hardness of 56 HRC |
Bohler-Uddeholm UDDEHOLM HOTVAR® Hot Work Tool Steel Molybdenum-vanadium alloyed steelHotvar® is a premium hot work steel developed by Uddeholm to provide very good performance in tooling up to 1200°F (650°C). The alloying elements in Hotvar® are .. |
|||
Modulus of Elasticity | 180 GPa @Temperature 399 °C |
26100 ksi @Temperature 750 °F |
hardness of 45 HRC |
Bohler-Uddeholm UDDEHOLM ORVAR® SUPREME (Premium AISI H13) Hot Work Tool Steel Chromium-molybdenum-vanadium alloyed steelA premium Cr-Mo-V-alloyed hot work die steel with good resistance to thermal fatigue. The steel is produced by a special melting and refining technique in o.. |
|||
Modulus of Elasticity | 180 GPa @Temperature 400 °C |
26100 ksi @Temperature 752 °F |
|
Assab Steels ASSAB 88 Cold Work Steel ASSAB 88 (SLEIPNER) is a chromium-molybdenum-vanadium alloyed tool steel which is characterized by:Good wear resistanceGood chipping resistanceHigh compressive strengthHigh hardness (>60HRC) after h.. |
|||
Modulus of Elasticity | 180 GPa @Temperature 400 °C |
26100 ksi @Temperature 752 °F |
|
Assab Steels DIEVAR Hot Work Steel DIEVAR is a high performance chromium-molybdenum-vanadium alloyed hot work tool steel which offers a very good resistance to heat checking, gross checking, hot wear and plastic deformation. DIEVAR i.. |
|||
Modulus of Elasticity | 180 GPa @Temperature 300 °C |
26100 ksi @Temperature 572 °F |
|
Outokumpu LDX 2101® Duplex Stainless Steel Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone.. |