Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 18.0 GPa | 2610 ksi | |
Lehmann & Voss LUVOCOM® 1105-7442 PEEK, with carbon fiber, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts.High chemical resistance parts, hydrolysis resi.. |
|||
Modulus of Elasticity | 18.0 GPa | 2610 ksi | |
Lehmann & Voss LUVOCOM® 1105-8234 PEEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Dynam.. |
|||
Modulus of Elasticity | 18.0 GPa | 2610 ksi | |
Lehmann & Voss LUVOCOM® 1114-8364 PAEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Good friction and wear behaviour especially at increased temperatures.Electrically conduct.. |
|||
Modulus of Elasticity | 18.0 GPa | 2610 ksi | |
Lehmann & Voss LUVOCOM® 1301-7293/GN PPS, linear, with glass fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic.. |
|||
Modulus of Elasticity | 18.0 GPa | 2610 ksi | |
Lehmann & Voss LUVOCOM® 1301-7329/GY PPS, linear, with glass fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic.. |
|||
Modulus of Elasticity | 18.0 GPa | 2610 ksi | |
Lehmann & Voss LUVOCOM® 1301-7648/BK PPS, linear, with glass fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic.. |
|||
Modulus of Elasticity | 18.0 GPa | 2610 ksi | |
Lehmann & Voss LUVOCOM® 1-8490 Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.High dimensionally stab.. |
|||
Modulus of Elasticity | 18.0 GPa | 2610 ksi | |
Lehmann & Voss LUVOCOM® 19-8195/FR Polyamide 46, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Modulus of Elasticity | 18.0 GPa | 2610 ksi | |
Lehmann & Voss LUVOCOM® 50/CF/30 Polycarbonate, with carbon fiber Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Modulus of Elasticity | 18.0 GPa | 2610 ksi | |
Lehmann & Voss LUVOCOM® 50-7807 Polycarbonate, with carbon fiber and demolding aid Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Modulus of Elasticity | 18.0 GPa | 2610 ksi | |
Indium Corp. Indalloy 170 Pure Lead Information Provided by Indium Corporation |
|||
Modulus of Elasticity | 18.0 GPa | 2610 ksi | |
Lehmann & Voss LUVOCOM® 1106-8374 Polyether imide, with carbon fiber and PTFE Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.Hig.. |
|||
Modulus of Elasticity | 18.0 GPa @Thickness >=1.50 mm |
2610 ksi @Thickness >=0.0591 in |
24hr/23°C/50% RH; ISO 178; IEC/EN 60893-2 5.2 |
Elektro-Isola G-Etronax M Melamine, Glass Fabric Reinforcement, White, Sheets Description: Melamine-based composite material reinforced with glass fabric. High arc resistance and tracking resistance. Flame-resistant. Self-extinguishing.Information provided by Elektro-Isola |
|||
Modulus of Elasticity | 18.0 - 55.0 GPa | 2610 - 7980 ksi | at constant current |
ETREMA Products Terfenol-D Magnetostrictive Smart Material (Tb0.3Dy0.7Fe1.92) Terfenol-D is the commercial name for Tb0.3Dy0.7Fe1.92; a composition of material that exhibits giant magnetostriction.Magnetostriction is the phenomenon in which an applied magnetic field causes an.. |