Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 159 GPa | 23000 ksi | |
Pacific Sintered Materials FN-262-T(HT) High Strength Nickel Steel Powdered Metal High strength, good impact resistant material for mechanical components. Excellent hardenability.Equivalent MPIF Specification: FN-0408-155HTAll information provided by Pacific Sintered Metals. |
|||
Modulus of Elasticity | 159 GPa | 23000 ksi | |
Meehanite HS Heat Resisting Cast Iron Type HS compares very favorably from a strength standpoint with any heat resisting metal. Compositional adjustments are made to suit the exact service conditions. It machines easily and provides m.. |
|||
Modulus of Elasticity | 159 GPa @Temperature 600 °C |
23100 ksi @Temperature 1110 °F |
|
Haynes HR-120® alloy, solution heat-treated Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Modulus of Elasticity | 159 GPa @Temperature 600 °C |
23100 ksi @Temperature 1110 °F |
|
Haynes HR-120® alloy, solution heat-treated aged at 1200°F for 1000 hours Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Modulus of Elasticity | 159 GPa @Temperature 600 °C |
23100 ksi @Temperature 1110 °F |
|
Haynes HR-120® alloy, solution heat-treated aged at 1400°F for 1000 hours Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Modulus of Elasticity | 159 GPa @Temperature 600 °C |
23100 ksi @Temperature 1110 °F |
|
Haynes HR-120® alloy, solution heat-treated aged at 1600°F for 1000 hours Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Modulus of Elasticity | 159 GPa @Temperature 600 °C |
23100 ksi @Temperature 1110 °F |
|
Haynes HR-120® alloy, solution heat-treated aged at 1800°F for 1000 hours Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Modulus of Elasticity | 159 GPa @Temperature 538 °C |
23000 ksi @Temperature 1000 °F |
|
Latrobe LSSâ„¢ H12 Hot Work Tool Steel (ASTM H12) TLS H12 hot work tool steel is a 5% chromium, general-purpose hot work steel that is characterized by excellent impact toughness. It contains less vanadium than the widely-used H13 hot work tool ste.. |
|||
Modulus of Elasticity | 159 GPa @Temperature 538 °C |
23000 ksi @Temperature 1000 °F |
|
Latrobe LSSâ„¢ H13 PQ Hot Work Tool Steel TLS H13 PQ is Premium Quality H13 hot work steel that is designed to meet the highest quality standards in the die casting industry, and to excel in the most demanding hot work tooling applications... |
|||
Modulus of Elasticity | 159 GPa @Temperature 538 °C |
23000 ksi @Temperature 1000 °F |
|
Latrobe LSSâ„¢ H13 Tool Steel (ASTM H13) TLS H13 tool steel is a versatile chromium-molybdenum hot work steel that is widely used in hot work and cold work tooling applications. The hot hardness (hot strength) of H13 resists thermal fatigu.. |
|||
Modulus of Elasticity | 159 GPa @Temperature 538 °C |
23000 ksi @Temperature 1000 °F |
|
Latrobe Viscount 20® Free Machining Tool Steel (ASTM H13S) Viscount 20 tool steel is a resulfurized H13 tool steel. The distribution of alloy sulfide particles in the microstructure enhances the machinability of the steel in the annealed condition. In addi.. |
|||
Modulus of Elasticity | 159 GPa @Temperature 700 °C |
23100 ksi @Temperature 1290 °F |
|
Haynes 718 alloy, cold rolled, solution-treated and aged sheet Cb and Ta content combined weight percentage of 5. Excellent high-temperature strength up to 650°C, good ductility, formability, and weldability. Very good welding characteristics. Applications i.. |
|||
Modulus of Elasticity | 159 GPa @Temperature 538 °C |
23000 ksi @Temperature 1000 °F |
|
Latrobe Dynaflex® VAC-ARC High Strength Alloy Steel DYNAFLEX VAC-ARC steel is a medium alloyed, air hardening ultra high strength grade designed for structural applications requiring room temperature tensile strengths of 220,000 to 300,000 psi. Due .. |
|||
Modulus of Elasticity | 159 GPa @Temperature 600 °C |
23100 ksi @Temperature 1110 °F |
|
Haynes HR-120® alloy, solution heat-treated plate Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Modulus of Elasticity | 159 GPa @Temperature 538 °C |
23000 ksi @Temperature 1000 °F |
|
Latrobe LSSâ„¢ H11 Hot Work Tool Steel (ASTM H11) TLS H11 hot work tool steel is a 5% chromium hot work steel that is characterized by excellent impact toughness. It contains less vanadium than the widely-used H13 hot work tool steel. This provides.. |
|||
Modulus of Elasticity | 159 GPa @Temperature 538 °C |
23000 ksi @Temperature 1000 °F |
|
Latrobe Viscount 44® Prehardened Tool Steel (ASTM H13S) Viscount 44 is a free-machining, prehardened, H13-type hot work tool steel. It is produced using special melting, forging, and heat treating processes which provide the optimum in control
and reprod.. |
|||
Modulus of Elasticity | 159 GPa @Temperature 649 °C |
23100 ksi @Temperature 1200 °F |
|
Haynes Multimet® alloy, 533.4 by 82.55 mm forging, stress relieved at 649°C (1200°F), air cooled Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductility, and i.. |
|||
Modulus of Elasticity | 159 GPa | 23000 ksi | |
Carpenter Glass Sealing "42-6" Alloy A nickel-chromium-iron which has been developed to match the thermal expansion characteristics of 0120 glass. An additional advantage of this alloy for glass-to-metals seals is the tight dark green.. |