Mechanical Properties Metric English Comments
Modulus of Elasticity 141 GPa

@Temperature 982 °C
20500 ksi

@Temperature 1800 °F
Haynes Hastelloy® C-4 alloy, all-weld metal, as welded, GTAW
Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) rang..
Modulus of Elasticity 141 GPa

@Temperature 982 °C
20500 ksi

@Temperature 1800 °F
Haynes Hastelloy® C-4 alloy, plate, heat treated at 1066°C, rapid quenched
Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) rang..
Modulus of Elasticity 141 GPa

@Temperature 982 °C
20500 ksi

@Temperature 1800 °F
Haynes Hastelloy® C-4 alloy, welded plate 12.7 mm (1/2 in.) thick, aged 1000 hours at 649°C (1200°F)
Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) rang..
Modulus of Elasticity 141 GPa

@Temperature 593 °C
20500 ksi

@Temperature 1100 °F
Crucible Steel 422 Stainless Steel
Crucible 422 is a hardenable martensitic stainless steel which is being widely used for high temperatures up to 1200°F. It has excellent creep-rupture properties in the range of 600/1200°F and is..
Modulus of Elasticity 141 GPa
20500 ksi
Carpenter Invar 36® Alloy, Annealed Bars and Strip
Data provided by Carpenter Technology Corporation.Carpenter Invar "36" alloy is a 36% nickel-iron alloy possessing a rate of thermal expansion approx. one-tenth that of carbon steel up to 200°C. T..
Modulus of Elasticity 141 GPa

@Temperature 982 °C
20500 ksi

@Temperature 1800 °F
Haynes Hastelloy® C-4 alloy, sheet, aged 100 hours at 899°C
Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) range. T..
Modulus of Elasticity 141 GPa

@Temperature 982 °C
20500 ksi

@Temperature 1800 °F
Haynes Hastelloy® C-4 alloy, sheet, heat treated at 1066°C, rapid quenched
Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) range. T..
Modulus of Elasticity 141 GPa

@Temperature 982 °C
20500 ksi

@Temperature 1800 °F
Haynes Hastelloy® C-4 alloy, welded plate 12.7 mm (1/2 in.) thick, aged 10 hours at 649°C (1200°F)
Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) range. T..
Modulus of Elasticity 141 GPa

@Temperature 982 °C
20500 ksi

@Temperature 1800 °F
Haynes Hastelloy® C-4 alloy, welded plate 12.7 mm (1/2 in.) thick, GTAW