Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 125 GPa | 18100 ksi | |
Osprey Metals CE7 Al-Si Controlled Expansion Alloy Si-30%Al controlled expansion alloy manufactured and patented by Osprey Metals Ltd.Information provided to MatWeb by Osprey Metals. |
|||
Modulus of Elasticity | 125 GPa | 18100 ksi | |
SGL Carbon Group SIGRAFIL C® in 250°F Epoxy 60% fiber volumeInformation provided by SGL Carbon Group |
|||
Modulus of Elasticity | 125 GPa | 18100 ksi | Typical |
TIMET 8-1-1 Titanium Alloy (Ti-8Al-1Mo-1V); Annealed Sheet Industry Specifications: USA Aerospace: AMS 4915,4916. France: T-A8DV. Features: Designed for creep resistance up to 450°C, used primarily in engine applications such as forged compressor blades.. |
|||
Modulus of Elasticity | 125 GPa | 18100 ksi | Typical |
TIMET TIMETAL® 685 (Ti-6Al-5Zr-0.5Mo-0.25Si) Titanium Alloy High-Temperature, High-Strength Creep Resistant AlloyIndustry Specifications: Germany Aerospace: 3.7154. France: T-A6ZD. UK Aerospace Specifications BS TA. 43, 44.Features: TIMETAL 685 possesses .. |
|||
Modulus of Elasticity | 125 GPa | 18100 ksi | UD |
UBE Tyrannohex® Heat Resistant Composite Description: Tyrannohex is a fiber assembled ceramic with both toughness like a shell or wood and excellent heat-resistance in air.Very high volume fraction (Vf) of the thin (~ 10m), continuous fibe.. |
|||
Modulus of Elasticity | 125 GPa | 18100 ksi | ASTM E494 |
M Cubed Technologies ASC-301 Aluminum alloy-30% SiC Metal Matrix Composite High stiffness, low density composite. Parts are cast using several standard foundry techniques Size range varies from small components (1lb or smaller) to parts greater than 10 ft. square with co.. |