Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 12.9 GPa | 1870 ksi | ASTM C580 |
Chesterton ARC 791 Composite Description: A quartz reinforced composite designed to resurface and restore concrete surfaces, to protect new concrete, and to repair concrete damaged by chemical and physical abuse. ARC 791 has ex.. |