Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Modulus of Elasticity = 113.8 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 113.8 GPa
16510 ksi
In rolling direction
AK Steel TRAN-COR® H-0 CARLITE® Grain Oriented Electrical Steel
TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l..
Modulus of Elasticity 113.8 GPa
16510 ksi
In rolling direction
AK Steel TRAN-COR® H-1 CARLITE® DR® Grain Oriented Electrical Steel
TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l..
Modulus of Elasticity 113.8 GPa
16510 ksi
In rolling direction
AK Steel TRAN-COR® H-1 CARLITE® Grain Oriented Electrical Steel
TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l..
Modulus of Elasticity 113.8 GPa
16510 ksi
In rolling direction
AK Steel TRAN-COR® H-2 CARLITE® DR® Grain Oriented Electrical Steel
TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l..
Modulus of Elasticity 113.8 GPa
16510 ksi
In rolling direction
AK Steel TRAN-COR® H-2 CARLITE® Grain Oriented Electrical Steel
TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l..
Modulus of Elasticity 113.8 GPa

@Temperature 649 °C
16510 ksi

@Temperature 1200 °F
Carpenter No. 883® Hot Work Die Steel (Red-Tough) (AISI H13)
No. 883 hot work die steel is a 5% chromium hot work tool steel designed particularly for applications requiring extreme toughness combined with good red-hardness. It has given an extra margin of sa..
Modulus of Elasticity 113.8 GPa
16510 ksi
In rolling direction
AK Steel TRAN-COR® H-0 CARLITE® DR® Grain Oriented Electrical Steel
TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l..
Copyright © lookpolymers.com All Rights Reserved