Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 1.86 GPa | 270 ksi | ASTM D-638 |
Plaskolite Optix® CA - 2000 HF-4-2 High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Modulus of Elasticity | 1.86 GPa | 270 ksi | ASTM D-638 |
Plaskolite Optix® CA - 2000 High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Modulus of Elasticity | 1.86 GPa | 270 ksi | ASTM D-638 |
Plaskolite Optix® CP - 1000 IG High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Modulus of Elasticity | 1.86 GPa | 270 ksi | ASTM D-638 |
Plaskolite West Optix® CP - 1000 IG High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |
|||
Modulus of Elasticity | 1.86 - 3.10 GPa | 270 - 450 ksi | Average value: 2.80 GPa Grade Count:8 |
Overview of materials for Acrylic, High Flow, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, High Flow, Molded". Each property range of values reported is minimum and maximum values of app.. |
|||
Modulus of Elasticity | 1.86 GPa | 270 ksi | Tangent; ASTM D790 |
Mitsui TPX® MBZ230 Methylpentene Copolymer, Filled, Opaque Grade
(discontinued **) TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi.. |
|||
Modulus of Elasticity | 1.86 - 8.96 GPa | 270 - 1300 ksi | Average value: 2.71 GPa Grade Count:14 |
Overview of materials for Nylon 612 with PTFE Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612 with PTFE Filler". Each property range of values reported is minimum and maximum values of app.. |
|||
Modulus of Elasticity | 1.86 GPa | 270 ksi | ASTM D-638 |
Plaskolite West Optix® CA - 2000 HF-4-2 High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |
|||
Modulus of Elasticity | 1.86 GPa | 270 ksi | ASTM D-638 |
Plaskolite West Optix® CA - 2000 High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |