Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 1.35 GPa | 196 ksi | 50% RH |
Murtfeldt Murylon® HT Nylon 46 The use of this highly temperature resistant polyamide enables reliable operation up to a constant service temperature of 155°C . The material retains its rigidity and creep strength over the entir.. |
|||
Modulus of Elasticity | 1.35 - 1.79 GPa | 196 - 260 ksi | Average value: 1.59 GPa Grade Count:15 |
Overview of materials for Polypropylene, Fiber Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Fiber Grade". Each property range of values reported is minimum and maximum values of app.. |
|||
Modulus of Elasticity | 1.35 - 8.96 GPa | 196 - 1300 ksi | Average value: 4.18 GPa Grade Count:87 |
Overview of materials for Nylon 6, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Bead Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Modulus of Elasticity | 1.35 GPa | 196 ksi | ISO R527 |
Arkema Group Orgalloy® LE 60 SF Polyamide Alloy Polyamide Alloy, Film and PackagingInformation provided by Arkema Group |
|||
Modulus of Elasticity | 1.35 GPa | 196 ksi | ISO 178 |
Addiplast Addilene H 140 Polypropylene Homopolymer Unreinforced, low flow for injection and extrusion, very translucentInformation provided by Addiplast. |
|||
Modulus of Elasticity | 1.35 GPa | 196 ksi | ISO 178 |
Addiplast Addilene H 652 Polypropylene Homopolymer High temperature resistance, high gloss, very good surface appearanceInformation provided by Addiplast. |