Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.950 GPa | 138 ksi | |
Murtfeldt Material ”S”® 1000 Black Antistatic Polyethylene, Conductive Material ”S”® 1000 is exclusively produced from ultra-high molecular weight polyethylene powder that is mixed with finely milled Original Material ”S”®. The fine milled material is compressio.. |
|||
Modulus of Elasticity | 0.950 GPa | 138 ksi | |
Murtfeldt Material ”S”® 1000 Green Polyethylene Material ”S”® 1000 is exclusively produced from ultra-high molecular weight polyethylene powder that is mixed with finely milled Original Material ”S”®. The fine milled material is compressio.. |
|||
Modulus of Elasticity | 0.950 - 3.23 GPa | 138 - 468 ksi | Average value: 2.11 GPa Grade Count:43 |
Overview of materials for Acetal Homopolymer, Unreinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced, Impact Grade". Each property range of values reported is minimum and m.. |
|||
Modulus of Elasticity | 0.950 - 3.79 GPa | 138 - 550 ksi | Average value: 2.89 GPa Grade Count:192 |
Overview of materials for Acrylic, General Purpose, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values .. |
|||
Modulus of Elasticity | 0.950 GPa | 138 ksi | ISO 178 |
Addiplast Addilene J 110 Polypropylene Copolymer UnreinforcedInformation provided by Addiplast. |
|||
Modulus of Elasticity | 0.950 GPa | 138 ksi | ISO 178 |
Addiplast Addilene J 370 Polypropylene Copolymer High impact strength, high elongation at breakInformation provided by Addiplast. |
|||
Modulus of Elasticity | 0.950 - 5.40 GPa | 138 - 783 ksi | Average value: 2.41 GPa Grade Count:147 |
Overview of materials for Polypropylene, Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |