Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.900 - 3.50 GPa | 131 - 508 ksi | Average value: 1.83 GPa Grade Count:35 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend". Each property range of values reported is minimum an.. |
|||
Modulus of Elasticity | 0.900 GPa | 131 ksi | 1 mm/min; ISO 527 |
Borealis Beta-PPR™ RA7050 Polypropylene-Random-Copolymer for Pressure Pipe Systems Beta-PPR RA7050 is a PP-RCT, a Polypropylene-Random-Copolymer with an enhanced Crystalline structure brought about by a special ß-nucleation and with an improved Temperature resistance. Proof of t.. |
|||
Modulus of Elasticity | 0.900 GPa | 131 ksi | 1 mm/min; ISO 527 |
Borealis Beta-PPR™ RA7050-GN Polypropylene-Random-Copolymer for Pressure Pipe Systems Beta-PPR RA7050-GN is a PP-RCT, a Polypropylene-Random-Copolymer with an enhanced Crystalline structure brought about by a special ß-nucleation and with an improved Temperature resistance. Proof o.. |
|||
Modulus of Elasticity | 0.900 GPa | 131 ksi | ISO 527 |
DSM Fibre Intermediates Nyrim® 1500 (Conditioned) Conditioned at 23°C and 50% Relative Humidity.Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is proc.. |
|||
Modulus of Elasticity | 0.900 GPa | 131 ksi | ISO 527-1/-2 |
BASF Ultramid® B3L BK00464 PA6 (Conditioned) Description: Impact-modified, free-flowing and rapidly processable injection-molding grade for dry impact-resistant technical articles such as, for example, housings, fittings, small parts and wall .. |
|||
Modulus of Elasticity | 0.900 - 1.20 GPa | 131 - 174 ksi | |
Biomer P209 PHB Biodegradable Polymer PHB is a isotactic, absolutely linear, thermoplastic homopolyester built of 3-hydroxy butyric acid. The formula of the subunit is -[O-CH(CH3)-CH2-CO]-. PHB is free from even traces of catalysts. P.. |
|||
Modulus of Elasticity | 0.900 GPa | 131 ksi | ISO 527 |
BASF Ultramid® B3L PA6 (Conditioned) Ultramid B3L is an impact-modified, easy flowing injection molding PA6 grade for fast processing. |
|||
Modulus of Elasticity | 0.900 GPa | 131 ksi | Conditioned; ISO 178 |
Addiplast Addinyl B2 Nylon 6 Unreinforced, medium viscosityInformation provided by Addiplast. |
|||
Modulus of Elasticity | 0.900 - 2.65 GPa | 131 - 384 ksi | Average value: 1.74 GPa Grade Count:36 |
Overview of materials for Acetal Copolymer, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Impact Modified". Each property range of values reported is minimum and maximum values.. |
|||
Modulus of Elasticity | 0.900 - 2.14 GPa | 131 - 310 ksi | Average value: 1.38 GPa Grade Count:15 |
Overview of materials for Polypropylene with 10% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be.. |