Modulus of Elasticity 0.700 GPa
102 ksi
Murtfeldt Material ”S”® 8000 Polyethylene
Material ”S”® 8000 improves on the already impressive material properties of Original Material ”S”®. The self lubricating character of this material makes it ideally suited for use in sliding..
Modulus of Elasticity 0.700 GPa
102 ksi
Murtfeldt Original Material ”S”® Black Antistatic Polyethylene, Conductive
Original Material ”S”® black has the same properties as Original Material ”S”® green/natural. In addition, it is also electrostatically conductive due to the addition of additives. Special Pro..
Modulus of Elasticity 0.700 GPa
102 ksi
Murtfeldt Original Material ”S”® Green Polyethylene
Material ”S”® is based on virgin, ultrahigh molecular weight low pressure polyethylene and significantly exceeds the requirements of DIN 16972. In particular, Material ”S”® green has excellen..
Modulus of Elasticity 0.700 GPa
102 ksi
Murtfeldt Original Material ”S”® Natural Polyethylene
Material ”S”® is based on virgin, ultrahigh molecular weight low pressure polyethylene and significantly exceeds the requirements of DIN 16972. In particular, Material ”S”® natural has excell..
Modulus of Elasticity 0.700 GPa
102 ksi
Murtfeldt Original Material ”S”® plus + AB Polyethylene, Antibacterial
Material ”S”® plus + AB contains special substances that prevent the growth of bacteria and other microbes. The material is thus ideally suited for use when manufacturing and processing foods.Sp..
Modulus of Elasticity 0.700 GPa
102 ksi
Murtfeldt Original Material ”S”® plus + FP Polyethylene
Original Material ”S”® plus+ FP [FS] is a technical plastic that completely meets the requirements of the food sector for the detectability of plastic foreign bodies in foods. “FP” stands for “..
Modulus of Elasticity 0.700 GPa
102 ksi
Murtfeldt Original Material ”S”® plus + GB Polyethylene, Glass Bead Filled
The balanced quantity of micro glass beads in Material ”S”® plus+ GB provides the combined benefits of extremely high molecular weight polyethylene and glass. The glass beads that protrude from ..
Modulus of Elasticity 0.700 GPa
102 ksi
Murtfeldt Original Material ”S”® plus + LF ESD Polyethylene, Low Friction Conductive
This material is electrically conductive and has half the sliding friction coefficient of the Original Material ”S”® enabling voltage to be dissipated at maximum speed with the same maximum frict..
Modulus of Elasticity 0.700 GPa
102 ksi
Murtfeldt Original Material ”S”® plus + LF Polyethylene, Low Friction
This material has half the sliding friction coefficient of the Original Material ”S”®. This enables an increased machine running speed at the same time as less abrasion and thus a lower maintenan..
Modulus of Elasticity 0.700 GPa
102 ksi
Murtfeldt Original Material ”S”® plus + TLS Polyethylene
Original Material ”S”® plus+ TLS is designed for high temperature industrial applications for which Original Material ”S”® could previously not be used. The thermal oxidation point has been i..
Modulus of Elasticity 0.700 GPa
102 ksi
1 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 61010 PVDF Copolymer  (discontinued **)
Key features of this grade: Permanent Plasticizing, Fuel Line, Piping, Formulated. Recommended processing is extrusion. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF i..
Modulus of Elasticity 0.700 - 13.6 GPa
102 - 1970 ksi
Average value: 4.94 GPa Grade Count:33
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Glass fiber Filled". Each property range of values reported is minimum..
Modulus of Elasticity 0.700 - 5.00 GPa
102 - 725 ksi
Average value: 2.51 GPa Grade Count:195
Overview of materials for Nylon 66, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
Modulus of Elasticity 0.700 GPa
102 ksi
ISO 178
Total 3802 B HDPE, cable, sheet, pipe, injection molding
FINATHENE® 3802 B is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low-pressure slurry polymerization process. FINATHENE® 3802 B is a black polyethylene..
Modulus of Elasticity 0.700 GPa
102 ksi
ISO 178
Total 3802 Blue MDPE pipe, injection molding
FINATHENE® 3802 Blue is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low pressure slurry polymerization process. FINATHENE® 3802 Blue is a blue polyeth..
Modulus of Elasticity 0.700 GPa
102 ksi
ISO 178
Total 3802 YCF MDPE pipe grade
FINATHENE® 3802 Y CF is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low pressure slurry polymerization process. FINATHENE® 3802 Y CF is a yellow cadmi..
Modulus of Elasticity 0.700 GPa
102 ksi
ISO R527
Arkema Group Orgalloy® LE 60 LM Polyamide Alloy
Polyamide Alloy, Film and PackagingInformation provided by Arkema Group
Modulus of Elasticity 0.700 GPa
102 ksi
Conditioned; ISO 178
Addiplast Addinyl B2 R Nylon 6
High impact resistanceInformation provided by Addiplast.
Modulus of Elasticity 0.700 - 1.00 GPa
102 - 145 ksi
Alliance BCN-11 Bonded (Composite) Magnetic Material
Modulus of Elasticity 0.700 - 1.00 GPa
102 - 145 ksi
Alliance BCN-13 Bonded (Composite) Magnetic Material
Modulus of Elasticity 0.700 GPa
102 ksi
Conditioned; ISO 178
Addiplast Addinyl PMD 20143 Nylon 6
High impact resistanceInformation provided by Addiplast.
Modulus of Elasticity 0.700 - 1.00 GPa
102 - 145 ksi
Alliance BCN-10 Bonded (Composite) Magnetic Material
Modulus of Elasticity 0.700 - 1.00 GPa
102 - 145 ksi
Alliance BCN-12 Bonded (Composite) Magnetic Material
Modulus of Elasticity 0.700 - 1.00 GPa
102 - 145 ksi
Alliance BCN-14 Bonded (Composite) Magnetic Material
Modulus of Elasticity 0.700 - 1.00 GPa
102 - 145 ksi
Alliance BCN-15 Bonded (Composite) Magnetic Material
Modulus of Elasticity 0.700 - 1.34 GPa
102 - 195 ksi
Average value: 0.961 GPa Grade Count:20
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Pipe Grade". Each property range of values reported is minimum and max..
Modulus of Elasticity 0.700 - 1.00 GPa
102 - 145 ksi
Alliance BCN-17 Bonded (Composite) Magnetic Material