Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | >= 0.650 GPa | >= 94.3 ksi | ISO 527-1 |
Orbilan ORBILAN® PE 1000 UHMW-PE Orbilan PE 1000 plastics distinguish themselves through their optimal balance of the technical features with regard to wear-resistance and impact resistance. The areas of use range from general mac.. |
|||
Modulus of Elasticity | 0.650 - 2.07 GPa | 94.3 - 300 ksi | Average value: 1.26 GPa Grade Count:23 |
Overview of materials for High Density Polyethylene (HDPE), Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Blow Molding Grade". Each property range of values reported is minimum.. |
|||
Modulus of Elasticity | 0.650 - 2.00 GPa @Temperature 60.0 - 150 °C |
94.3 - 290 ksi @Temperature 140 - 302 °F |
Average value: 1.15 GPa Grade Count:1 |
Overview of materials for Nylon 66/6 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6". Each property range of values reported is minimum and maximum values of appropriate MatWeb .. |
|||
Modulus of Elasticity | 0.650 GPa | 94.3 ksi | |
AorTech Biomaterials Elast-Eon™ E2-862 Biomedical Polyurethane Pellets Elast-Eon™ polymers are used in biomedical applications. They have high biostability so they can be used for long term implantation. |
|||
Modulus of Elasticity | 0.650 GPa | 94.3 ksi | |
AorTech Biomaterials Elast-Eon™ E2-862 Biomedical Polyurethane Pellets Elast-Eon™ polymers are used in biomedical applications. They have high biostability so they can be used for long term implantation. |
|||
Modulus of Elasticity | 0.650 - 1.10 GPa @Temperature 60.0 - 90.0 °C |
94.3 - 160 ksi @Temperature 140 - 194 °F |
Average value: 0.875 GPa Grade Count:1 |
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and .. |