Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.390 - 0.750 GPa | 56.6 - 109 ksi | Average value: 0.599 GPa Grade Count:3 |
Overview of materials for Polytetrafluoroethylene (PTFE), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Extruded". Each property range of values reported is minimum and maximum.. |
|||
Modulus of Elasticity | 0.390 - 0.600 GPa | 56.6 - 87.0 ksi | ASTM D638 |
Zeus PTFE Tubing Zeus offers a wide range of standard size products and precision custom PTFE Tubing. PTFE Tubing has become the gold standard in industries requiring the ultimate in lubricity, high temperature use,.. |