Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.300 - 1.30 GPa | 43.5 - 189 ksi | Average value: 0.720 GPa Grade Count:75 |
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i.. |
|||
Modulus of Elasticity | 0.300 GPa | 43.5 ksi | |
Lehmann & Voss LUVOCOM® 94-8485 LD-PE, unreinforced Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Reduced moment of inertia compared with metal parts.Dynamic stressed parts.Especially suitable .. |
|||
Modulus of Elasticity | 0.300 GPa @Temperature 23.0 °C |
43.5 ksi @Temperature 73.4 °F |
MD/TD; ASTM D638 |
Mapal Plastics Maplon Type O Polypropylene Sheet Properties: Corona treated on both sides for offset and screen printing, Extended shelf life, Low stress whitening, Suitable for die cuttingApplications: Stationery products, Offset printed item |
|||
Modulus of Elasticity | 0.300 GPa @Temperature 23.0 °C |
43.5 ksi @Temperature 73.4 °F |
MD/TD; ASTM D638 |
Mapal Plastics Maplon Type S Polypropylene Sheet Properties: Low stress whitening, Suitable for die cutting, Corona treated on both sides for offset and screen printingApplications: Stationery, Packaging, House-hold productsand printed items |
|||
Modulus of Elasticity | 0.300 GPa | 43.5 ksi | ASTM D638 |
ITW Plexus Plexusâ„¢ AO420FS Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies. |
|||
Modulus of Elasticity | 0.300 GPa | 43.5 ksi | ISO R527 |
Arkema Group Orgalloy® LT 4060 ES Polyamide Alloy Polyamide Alloy, Blow Molding of Technical PartsInformation provided by Arkema Group |
|||
Modulus of Elasticity | 0.300 GPa | 43.5 ksi | ISO R527 |
Arkema Group Orgalloy® LT 4060 Polyamide Alloy Polyamide Alloy, Flexible gradeTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group |
|||
Modulus of Elasticity | 0.300 - 0.550 GPa @Temperature 60.0 - 150 °C |
43.5 - 79.8 ksi @Temperature 140 - 302 °F |
Average value: 0.379 GPa Grade Count:1 |
Overview of materials for Nylon 6, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro.. |
|||
Modulus of Elasticity | 0.300 - 5.70 GPa @Temperature 60.0 - 90.0 °C |
43.5 - 827 ksi @Temperature 140 - 194 °F |
Average value: 1.26 GPa Grade Count:8 |
Overview of materials for Polypropylene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of.. |
|||
Modulus of Elasticity | 0.300 GPa | 43.5 ksi | ASTM D638 |
ITW Plexus Plexus™ MA440 Methacrylate Adhesive Two-part, self-leveling adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies. |
|||
Modulus of Elasticity | 0.300 GPa | 43.5 ksi | ISO 5527 |
Total Lacqtene® 1025 FH 24 LDPE blown film
(discontinued **) Radical polyethylene made by high pressure tubular process. Slip and antiblock formulated grade for good transparent thin films. Advised temperature profile : 150 to 190°C.Information provided prov.. |