Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.260 GPa | 37.7 ksi | (stiffness), ASTM D882 |
DuPont™ Clysar® ABL Polyolefin Shrink Packaging Film, 60 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat shrinkable, linear low/ultra low density polyolefin film. Used where lower processing temperatures, superior pack.. |
|||
Modulus of Elasticity | 0.260 GPa | 37.7 ksi | (stiffness), ASTM D882 |
DuPont™ Clysar® ABL Polyolefin Shrink Packaging Film, 75 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat shrinkable, linear low/ultra low density polyolefin film. Used where lower processing temperatures, superior pack.. |
|||
Modulus of Elasticity | 0.260 GPa | 37.7 ksi | (stiffness), ASTM D882 |
DuPont™ Clysar® ABL Polyolefin Shrink Packaging Film, 100 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat shrinkable, linear low/ultra low density polyolefin film. Used where lower processing temperatures, superior pack.. |
|||
Modulus of Elasticity | 0.260 GPa | 37.7 ksi | TD; ISO R527-1 |
Iran Petrochemical (PCC) 2602TH00 Low Density Polyethylene LDPE 2602TH00 high clarity film Applications: film, underblankets and films for medical applications.Information provided by Iran Petrochemical Commercial Co. |
|||
Modulus of Elasticity | 0.260 GPa | 37.7 ksi | ASTM D638 |
Arkema Group Pebax® 6333 Polyether Block Amide (PEBA) Information provided by Arkema Group |
|||
Modulus of Elasticity | 0.260 GPa | 37.7 ksi | (stiffness), ASTM D882 |
DuPont™ Clysar® ABL Polyolefin Shrink Packaging Film, 125 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat shrinkable, linear low/ultra low density polyolefin film. Used where lower processing temperatures, superior pack.. |