Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.200 GPa | 29.0 ksi | ISO 178 |
Premix Thermoplastics PRE-ELEC® CP 1315
(discontinued **) PRE-ELEC CP 1315 is a conductive thermoplastic compound based on a polyolefin copolymer. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivit.. |
|||
Modulus of Elasticity | 0.200 GPa | 29.0 ksi | 1 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 32008 PVDF Copolymer
(Unverified Data**) Key features of this grade: High Flexibility/ High Elongation/Cold Impact Resistance, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General .. |
|||
Modulus of Elasticity | 0.200 GPa | 29.0 ksi | TD; ISO R527-1 |
Iran Petrochemical (PCC) 2102TX00 Low Density Polyethylene LDPE 2102TX00 GP filmIt is used in wide range of widths and thicknesses e.g. for punches, bags, liners and lamination film.Information provided by Iran Petrochemical Commercial Co. |
|||
Modulus of Elasticity | 0.200 GPa | 29.0 ksi | TD; ISO R527-1 |
Iran Petrochemical (PCC) 2501TN00 Low Density Polyethylene LDPE 2501TN00 Hygienic Film It is used in diaper film, lamination film and in applications where low blocking behavior without the help of additives is required.Information provided by Iran Petroch.. |
|||
Modulus of Elasticity | 0.200 GPa | 29.0 ksi | |
Lehmann & Voss LUVOCOM® TPE-7711/GY Thermoplastic elastomer, with carbon fiber, electrically conducting Applications: Electrically conductive, suitable for continuous discharging of statically generated electricity.Dynamic stressed parts.Bearings, sleeves, sliding elements, chair rollers, handles.Info.. |
|||
Modulus of Elasticity | 0.200 GPa | 29.0 ksi | TD; ISO 527 |
Iran Petrochemical (PCC) LL0209AA Linear Low Density Polyethylene LL 0209AA is a LLDPE copolymer with butene as comonomer which contains anti-oxidant. It is recommended for general purpose applications.Information provided by Iran Petrochemical Commercial Co. |
|||
Modulus of Elasticity | >= 0.200 GPa | >= 29.0 ksi | TM-019E |
AorTech Biomaterials Elast-Eon™ E2-852 Biomedical Polyurethane Pellets Elast-Eon™ 2-852 is a polyurethane with a 52% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in DM.. |
|||
Modulus of Elasticity | >= 0.200 GPa | >= 29.0 ksi | TM-019E |
AorTech Biomaterials Elast-Eon™ E2-852 Biomedical Polyurethane Pellets Elast-Eon™ 2-852 is a polyurethane with a 52% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in DM.. |
|||
Modulus of Elasticity | 0.200 - 0.300 GPa | 29.0 - 43.5 ksi | Average value: 0.220 GPa Grade Count:7 |
Overview of materials for Low Density Polyethylene (LDPE), Wire/Cable Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Wire/Cable Grade". Each property range of values reported is minimum an.. |
|||
Modulus of Elasticity | 0.200 - 2.20 GPa | 29.0 - 319 ksi | Average value: 1.02 GPa Grade Count:20 |
Overview of materials for Nylon, Flexible Alloy This property data is a summary of similar materials in the MatWeb database for the category "Nylon, Flexible Alloy". Each property range of values reported is minimum and maximum values of appropri.. |