Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.160 GPa | 23.2 ksi | MD; ISO R527-1 |
Iran Petrochemical (PCC) 2101TN47 Low Density Polyethylene LDPE 2101TN47 Shrink FilmThis grade enables high speed production of film without blocking.Information provided by Iran Petrochemical Commercial Co. |
|||
Modulus of Elasticity | 0.160 GPa | 23.2 ksi | MD; ISO 527 |
Iran Petrochemical (PCC) LS0085/KJ Low Density Polyethylene LS0085/KJ is a high molecular weight low density polyethylene film grade combining good flexible extrusion behavior and superior mechanical properties.Application: shrink packaging.Information prov.. |
|||
Modulus of Elasticity | 0.160 GPa | 23.2 ksi | ISO 527-2 |
Total EVA 1005 VN 2 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1005 VN 2 is made by a high pressure tubular process. Grade for transparent and resistant films. Contains an antioxidant.Application examples: Stretch, coextrusion, frozen food, agriculture fi.. |
|||
Modulus of Elasticity | 0.160 GPa | 23.2 ksi | ISO 527-2 |
Total LDPE 1200 MN 18 C Low Density Polyethylene - Injection Molding and Compounding LDPE 1200 MN 18 C is a low density polyethylene made by a high pressure autoclave process without antioxidant.Application examples: flexible molding, handles, closures, household items, toys, variou.. |
|||
Modulus of Elasticity | 0.160 - 0.442 GPa | 23.2 - 64.1 ksi | Average value: 0.240 GPa Grade Count:71 |
Overview of materials for Low Density Polyethylene (LDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Film Grade". Each property range of values reported is minimum and maxi.. |