Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.109 - 12.1 GPa @Temperature -40.0 - 150 °C |
15.8 - 1750 ksi @Temperature -40.0 - 302 °F |
Average value: 2.88 GPa Grade Count:7 |
Overview of materials for Nylon 610 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |