Polymer Property : Modulus of Elasticity = 0.0370 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.0370 GPa
5.37 ksi
DuPont Elvax® 450 Ethylene-Vinyl Acetate Copolymer Resin
Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with..
Modulus of Elasticity 0.0370 - 42.0 GPa
5.37 - 6090 ksi
Average value: 7.22 GPa Grade Count:739
Overview of materials for Polyetherimide (PEI)
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide". Each property range of values reported is minimum and maximum values of appropriate Mat..