Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.0170 GPa | 2.47 ksi | ISO 527 |
Lucobit Lucobit® 1210 Ethylene Copolymer Bitumen Lucobit® combines the positive properties of polyolefins and bitumen. The material is black and consists of mixtures based on high quality polyethylene copolymers with varying additions of speci.. |
|||
Modulus of Elasticity | 0.0170 GPa | 2.47 ksi | |
Lucobit Lucobit® 1210A Ethylene Copolymer Bitumen Lucobit 1210A is a mixture of ethylene copolymers and special bitumen. Addition of Lucobit to bitumen increases its viscosity and broadens the range of plasticity.Lucobit 1210A in asphalt mixtures .. |