Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.0138 - 6.00 GPa | 2.00 - 870 ksi | Average value: 2.34 GPa Grade Count:65 |
Overview of materials for Epoxy Encapsulant, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Encapsulant, Unreinforced". Each property range of values reported is minimum and maximum values o.. |
|||
Modulus of Elasticity | 0.0138 GPa | 2.00 ksi | ASTM D412 Method A |
Seals Eastern 7336 Highly Saturated Nitrile Rubber HNBR for Oil & Gas serviceInformation provided by Seals Eastern, Inc. |