Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.00860 GPa | 1.25 ksi | ASTM D638 |
ExxonMobil Escor® AT-320 EMAAA Terpolymer for Polymer Modification
(discontinued **) Data provided by the manufacturer, Exxon Chemical.45 Acid Number. Provides unusual adhesion to a variety of substrates and other components, such as aluminum foil, polyolefins, polycarbonate, PET, .. |